- 1. Clean the basis of the wounded area with a cleanser to collect grease and residue.
- 2. Open the wound with a round head scrubber.
- 3. Clean the workpiece with a solution.
- 4. Apply paint onto the workpiece according to the damaged condition for 3-4 times. For tint to adhere to the workpiece.
- 5. Bake tinted with infrared machine, heat to 70-80 degrees and let the tint to cool down.
- 6. Scrub open the tinting face and smooth out the tinted skin. And clean the scrub areas.
- 7. Apply 2-3 coats of primer to prevent the floor paint from frustrating. Each trip has to be abandoned during 2-3 minutes.
- 8. Bake the primer in the baking room for 12 minutes.
- 9. Scrub the face, open the primer. And check the smoothness.
- 10. Use a blow gun to clean. And wipe clean with liquid.
- 11. Use light to Day Light brightness 1500 Luk to check the smoothness of the workpiece.
- 12. The first real paint By covering the workpiece before 50-70%
- 13. Second time actually spraying By covering the work piece 100%
- 14. Check to see if the color matches the desired color.
- 15. Drying at 60 degrees for 30 minutes or infrared 10 minutes.
- 16. Spray paint to cover the work piece 2 times.
- 17. Wait for the workpiece to cool before taking it out of the pipe room. Polished with polish.
- 18. Inspect work before delivery.